Mekhanika Mikrostruktur: Effektivnye I Lokal'nye Svoystva Teksturirovannykh Polikristallov I Kompozitov - Viktor Yakovlev - Books - LAP LAMBERT Academic Publishing - 9783843324168 - May 24, 2011
In case cover and title do not match, the title is correct

Mekhanika Mikrostruktur: Effektivnye I Lokal'nye Svoystva Teksturirovannykh Polikristallov I Kompozitov Russian edition

Price
R 1,014
excl. VAT

Ordered from remote warehouse

Expected to be ready for shipping Nov 27 - Dec 3
Christmas presents can be returned until 31 January
Get notified about new Viktor Yakovlev releases
Add to your iMusic wish list

Not rated yet

V knige rassmotreny sovremennye predstavleniya o prognozirovanii effektivnykh i lokal'nykh fiziko- mekhanicheskikh kharakteristik teksturirovannykh polikristallov i kompozitov. Predstavleny rezul'taty issledovaniy avtorov o vliyanii sostava, struktury, orientatsii i kontsentratsii komponentov na uprugie svoystva neodnorodnykh materialov. Opisan provedennyy avtorami kompleksnyy teoreticheskiy analiz vzaimosvyazi effektivnykh i lokal'nykh uprugikh kharakteristik real'nykh polikristallicheskikh sred s usloviyami ikh formirovaniya, opirayushchiysya na neytrono- i rentgenograficheskie dannye o kristallograficheskoy teksture obraztsov. Predstavlen metod modelirovaniya teksturoobrazovaniya v polikristallakh pri prilozhenii razlichnykh vneshnikh napryazheniy, osnovannyy na analize lokal'noy plotnosti energii deformatsii. Udeleno vnimanie rezul'tatam chislennogo modelirovaniya effektivnykh uprugikh kharakteristik kompozitnykh geomaterialov s uchetom kristallograficheskoy tekstury komponentov. Dlya inzhenerno-tekhnicheskikh i nauchnykh sotrudnikov, rabotayushchikh v oblasti modelirovaniya, rascheta, proektirovaniya i sozdaniya teksturirovannykh polikristallov i kompozitov, a takzhe studentov i aspirantov sootvetstvuyushchikh spetsial'nostey.

Media Books     Paperback Book   (Book with soft cover and glued back)
Released May 24, 2011
ISBN13 9783843324168
Publishers LAP LAMBERT Academic Publishing
Pages 164
Dimensions 150 × 10 × 226 mm   ·   262 g
Language German